Nut flange type M8 Electro-Galv
Item number
CSU08891100
Local code:
*
GTIN:
8712186106545
Description:
Nut flange type M8 Electro-Galv
Wibe Group. CSU08891100 - Stago - nut flange type - M8 - electro-galvanized
Properties
Status product
Product status
Commercialized
Commercial and Web
Short description
Nut flange type M8 Electro-Galv
Medium description
Stago - nut flange type - M8 - electro-galvanized
Material
Steel
Material type or surface treatment
Electro-galvanized
Environmental corrosion class
C1
Base
Activity
Cable support systems
Product family
Common accessories
Brand
Stago
GTIN
8712186106545
ETIM (EC003863-Nut)
Model (EF000010)
*
With flange (EF005729)
*
Weldable (EF011770)
*
Self (EF006319)
*
With nylon ring (EF006024)
*
Screwing system (EF000013)
*
Material (EF002169)
Steel
Material quality (EF001257)
*
Active ingredient (EF013622)
*
Surface protection (EF000139)
*
Thread size (metric) (EF003563)
*
Thread size (imperial) (EF003715)
*
Wrench width (EF000177)
* mm
Pitch thread (EF003712)
* mm
Thread per inch (EF012132)
*
Thread type (EF001758)
*
Left (EF022707)
*
Height (EF000040)
* mm
Outer diameter (EF000015)
* mm
Colour (EF000007)
*
RAL (EF000116)
*
Halogen free (EF000025)
*
Logistic
Customs code
7318169290
Net weight
.01 kg
Country of origin
NL
Certification
ETIM class
EC003863
Product downloads
Environmental Documents
Downloads
Environmental Products
Corrosion class | C1 | C2 | C3 | C4 | C5 | CX | |
Environmental corrosion | Very low | Low | Average | High | Very high | Extreme | |
Examples of environments | Indoors | Heated areas with arid atmosphere and insignificant quantities of pollutant, e.g. offices, shops, schools and hotels. | Non-heated areas with fluctuating levels of temperature and humidity. Few instances of condensation and low levels of airborne pollution, e.g. sports halls and warehouses. | Average levels of humidity and some airborne pollution resulting from production processes, e.g. breweries, dairies, laundries. | High humidity and considerable airborne pollution as the result of production processes, e.g. chemical plants, swimming pools and dockyards. | Buildings with almost permanent condensation and with high pollution | Industrial buildings with extreme humidity and aggressive atmosphere. |
Outdoors | Atmospheres with low levels of airborne pollution. Rural areas. | Atmospheres containing some salt or average levels of air-borne pollution. Urban and light industrial areas. Areas affected by coastal conditions. | Atmospheres with average salt content or discernible levels of airborne pollution. Industrial and coastal areas. | Industrial areas with high humidity and aggressive atmosphere, and coastal areas with high salinity | Offshore areas with high salinity, industrial areas with extreme humidity, and aggressive atmospheres, sub-tropical or tropical atmospheres. | ||
Wibe Group designation
Exceeds requirements. Extremely high durability.
Recommended very high durability ( >20 years)
Possible alternative. High durability (10-20 years) |
Electro-galvanized (EG) |
|
|
||||
Pre-galvanized (PG) |
|
|
|
||||
Zinc+ (Z+) |
|
|
|
|
|||
Hot-dip galvanized (HDG) |
|
|
|
|
|
||
Zinkpox (ZP) |
|
|
|
|
|
|
|
Stainless steel AISI 304L(SS304) |
|
|
|
|
|
|
|
Stainless steel AISI 316L (SS316) |
|
|
|
|
|
|
|
Glass Fibre Reinforced Polymer (FRP/GRP) |
|
|
|
|
|
|
This table shows estimated values.
For more detailed advice, please contact technical support at Wibe Group