Bend Lokk 90o 50, PC1
El nummer
1331518
Artikkelnummer:
MCT3212PC1
GTIN:
7321678034078
Beskrivelse:
Bend Lokk 90o 50, PC1
Produktegenskaper
Status produkt
Produktstatus
Aktiv artikkel
Kommersiell og web
lokal kode (e-nr)
1331518
Vareteks
Bend Lokk 90o 50, PC1
Vareteks medium
Bend Lokk 90o 50, PC1
Lengde
440 mm
Bredde
440 mm
Høyde
12 mm
Materiale
GRP
Materialtype / overflatebehandling
PC1
Miljøkorrosjonsklasse
CX
Bas
Aktivitet
Kabelforleggning
Produktfamilie
Kabelrenner
Fabrikat
Mita
Serie
Flex
GTIN
7321678034078
ETIM (EC002402-Deksel til bøyer for kabelforleggingssystem)
Vinkel (verdi) (EF001218)
90°
Retningsendring (EF005210)
Horisontal
Bredde (EF000008)
50 mm
Lengde (EF001438)
* mm
Egnet for kabelrenne (EF005166)
Ja
Egnet for gitterrenne (EF005163)
Nei
Egnet for kabelstige (EF005165)
Nei
Type feste (EF002442)
Dekselklammer
Hengslet (EF001076)
Nei
Egnet for funksjonsopprettholdelse (EF007806)
Nei
Materiale (EF002169)
Andre
Materialkvalitet (EF001257)
GFK (glassfiberforsterket plast)
Overflatebeskyttelse (EF000139)
Andre
Farge (EF000007)
Grå
RAL (EF000116)
7047
Logistikk
Tolltariffnummer
39169010
Nettovekt
0,3 kg
Opprinnelsesland
Malaysia
Sertifisering
ETIM-klasse
EC002402
Produktnedlastinger
Environmental Documents
Corrosion class | C1 | C2 | C3 | C4 | C5 | CX | |
Environmental corrosion | Very low | Low | Average | High | Very high | Extreme | |
Examples of environments | Indoors | Heated areas with arid atmosphere and insignificant quantities of pollutant, e.g. offices, shops, schools and hotels. | Non-heated areas with fluctuating levels of temperature and humidity. Few instances of condensation and low levels of airborne pollution, e.g. sports halls and warehouses. | Average levels of humidity and some airborne pollution resulting from production processes, e.g. breweries, dairies, laundries. | High humidity and considerable airborne pollution as the result of production processes, e.g. chemical plants, swimming pools and dockyards. | Buildings with almost permanent condensation and with high pollution | Industrial buildings with extreme humidity and aggressive atmosphere. |
Outdoors | Atmospheres with low levels of airborne pollution. Rural areas. | Atmospheres containing some salt or average levels of air-borne pollution. Urban and light industrial areas. Areas affected by coastal conditions. | Atmospheres with average salt content or discernible levels of airborne pollution. Industrial and coastal areas. | Industrial areas with high humidity and aggressive atmosphere, and coastal areas with high salinity | Offshore areas with high salinity, industrial areas with extreme humidity, and aggressive atmospheres, sub-tropical or tropical atmospheres. | ||
Wibe Group designation
Exceeds requirements. Extremely high durability.
Recommended very high durability ( >20 years)
Possible alternative. High durability (10-20 years) |
Electro-galvanized (EG) |
|
|
||||
Pre-galvanized (PG) |
|
|
|
||||
Zinc+ (Z+) |
|
|
|
|
|||
Hot-dip galvanized (HDG) |
|
|
|
|
|
||
Zinkpox (ZP) |
|
|
|
|
|
|
|
Stainless steel AISI 304L(SS304) |
|
|
|
|
|
|
|
Stainless steel AISI 316L (SS316) |
|
|
|
|
|
|
|
Glass Fibre Reinforced Polymer (FRP/GRP) |
|
|
|
|
|
|
This table shows estimated values.
For more detailed advice, please contact technical support at Wibe Group