AFTAKHAAK 47 TV
Artikelnummer
791350
E-Nummer:
*
GTIN:
7321677913503
Omschrijving:
AFTAKHAAK 47 TV
Wibe Group. 791350 - Wibe - aftakhaak 47 - thermisch verzinkt
Eigenschappen
Status Product
Product status
Gecommercialiseerd
Product Omschrijving
Korte omschrijving
AFTAKHAAK 47 TV
Medium omschrijving
WIBE - Aftakhaak 47 - Thermisch verzinkt
Materiaal
Staal
Materiaaltype of oppervlaktebehandeling
Thermisch verzinkt
Milieu corrosieklasse
C4
Basis
Activiteit
Kabeldraagsystemen
Productfamilie
Ladderbanen
Merk
Wibe
GTIN
7321677913503
ETIM (EC000483-Verbindingselement profielrail)
Geschikt voor (EF000073)
*
Uitvoering (EF000010)
T-koppeling
Hoek (EF008153)
90 °
Met schroeftoebehoren (EF005067)
Nee
Materiaal (EF002169)
Staal
Roestvaststaal (RVS), gebeitst (EF006388)
Nee
Kwaliteitsklasse (EF001257)
Overig
Oppervlaktebescherming (EF000139)
EV001298
Aantal gaten/sleuven per zijde (EF023769)
2
In de rail (EF005902)
Nee
Op de rail (EF023768)
Ja
Logistiek
Aantal verpakking 1
1
Gewicht verpakking 1
,37 kg
Lengte verpakking 1
160 mm
Breedte verpakking 1
75 mm
Hoogte verpakking 1
20 mm
Douane code
73089059
Netto gewicht
,37 kg
Land van productie
SE
Certificering
ETIM classificatie
EC000483
Duurzaamheid
GWP Total A1-A3
1,0323 kgCO2e
Product downloads
Duurzaamheidsdocumenten
Downloads
Duurzaamheidsverklaringen
Corrosion class | C1 | C2 | C3 | C4 | C5 | CX | |
Environmental corrosion | Very low | Low | Average | High | Very high | Extreme | |
Examples of environments | Indoors | Heated areas with arid atmosphere and insignificant quantities of pollutant, e.g. offices, shops, schools and hotels. | Non-heated areas with fluctuating levels of temperature and humidity. Few instances of condensation and low levels of airborne pollution, e.g. sports halls and warehouses. | Average levels of humidity and some airborne pollution resulting from production processes, e.g. breweries, dairies, laundries. | High humidity and considerable airborne pollution as the result of production processes, e.g. chemical plants, swimming pools and dockyards. | Buildings with almost permanent condensation and with high pollution | Industrial buildings with extreme humidity and aggressive atmosphere. |
Outdoors | Atmospheres with low levels of airborne pollution. Rural areas. | Atmospheres containing some salt or average levels of air-borne pollution. Urban and light industrial areas. Areas affected by coastal conditions. | Atmospheres with average salt content or discernible levels of airborne pollution. Industrial and coastal areas. | Industrial areas with high humidity and aggressive atmosphere, and coastal areas with high salinity | Offshore areas with high salinity, industrial areas with extreme humidity, and aggressive atmospheres, sub-tropical or tropical atmospheres. | ||
Wibe Group designation
Exceeds requirements. Extremely high durability.
Recommended very high durability ( >20 years)
Possible alternative. High durability (10-20 years) |
Electro-galvanized (EG) |
|
|
||||
Pre-galvanized (PG) |
|
|
|
||||
Zinc+ (Z+) |
|
|
|
|
|||
Hot-dip galvanized (HDG) |
|
|
|
|
|
||
Zinkpox (ZP) |
|
|
|
|
|
|
|
Stainless steel AISI 304L(SS304) |
|
|
|
|
|
|
|
Stainless steel AISI 316L (SS316) |
|
|
|
|
|
|
|
Glass Fibre Reinforced Polymer (FRP/GRP) |
|
|
|
|
|
|