Klammer lokk Rf
El nummer
1357711
Artikkelnummer:
CSU08852000
GTIN:
8712186073786
Beskrivelse:
Klammer lokk Rf
Produktegenskaper
Status produkt
Produktstatus
Aktiv artikkel
Kommersiell og web
lokal kode (e-nr)
1357711
Vareteks
Klammer lokk Rf
Vareteks medium
Klammer lokk AISI301
Lengde
39 mm
Bredde
24 mm
Høyde
16 mm
Materiale
Stål
Materialtype / overflatebehandling
AISI301
Miljøkorrosjonsklasse
C2; C3; C4; C5
Bas
Aktivitet
Kabelforleggning
Produktfamilie
Tilbehør
Fabrikat
Stago
GTIN
8712186073786
ETIM (EC001002-Dekselklemme for kabelkanal)
Egnet for gitterrenne (EF005163)
Nei
Egnet for kabelstige (EF005165)
Nei
Egnet for kabelrenne (EF005166)
Ja
Materiale (EF002169)
Rustfritt stål
Rustfritt stål, beiset (EF006388)
Ja
Materialkvalitet (EF001257)
Andre
Overflatebeskyttelse (EF000139)
Andre
Logistikk
Tolltariffnummer
7308909800
Nettovekt
,01 kg
Opprinnelsesland
NL
Sertifisering
ETIM-klasse
EC001002
Produktnedlastinger
Environmental Documents
Nedlastninger
Environmental Products
Corrosion class | C1 | C2 | C3 | C4 | C5 | CX | |
Environmental corrosion | Very low | Low | Average | High | Very high | Extreme | |
Examples of environments | Indoors | Heated areas with arid atmosphere and insignificant quantities of pollutant, e.g. offices, shops, schools and hotels. | Non-heated areas with fluctuating levels of temperature and humidity. Few instances of condensation and low levels of airborne pollution, e.g. sports halls and warehouses. | Average levels of humidity and some airborne pollution resulting from production processes, e.g. breweries, dairies, laundries. | High humidity and considerable airborne pollution as the result of production processes, e.g. chemical plants, swimming pools and dockyards. | Buildings with almost permanent condensation and with high pollution | Industrial buildings with extreme humidity and aggressive atmosphere. |
Outdoors | Atmospheres with low levels of airborne pollution. Rural areas. | Atmospheres containing some salt or average levels of air-borne pollution. Urban and light industrial areas. Areas affected by coastal conditions. | Atmospheres with average salt content or discernible levels of airborne pollution. Industrial and coastal areas. | Industrial areas with high humidity and aggressive atmosphere, and coastal areas with high salinity | Offshore areas with high salinity, industrial areas with extreme humidity, and aggressive atmospheres, sub-tropical or tropical atmospheres. | ||
Wibe Group designation
Exceeds requirements. Extremely high durability.
Recommended very high durability ( >20 years)
Possible alternative. High durability (10-20 years) |
Electro-galvanized (EG) |
|
|
||||
Pre-galvanized (PG) |
|
|
|
||||
Zinc+ (Z+) |
|
|
|
|
|||
Hot-dip galvanized (HDG) |
|
|
|
|
|
||
Zinkpox (ZP) |
|
|
|
|
|
|
|
Stainless steel AISI 304L(SS304) |
|
|
|
|
|
|
|
Stainless steel AISI 316L (SS316) |
|
|
|
|
|
|
|
Glass Fibre Reinforced Polymer (FRP/GRP) |
|
|
|
|
|
|
This table shows estimated values.