CLX3 Wall Bracket
Item number
CSU795804
Local code:
*
GTIN:
7321677958047
Description:
CLX3 Wall Bracket
Wibe Group. CSU795804 - Wibe - Wall bracket for CLX3 cantilevers
Properties
Status product
Product status
Commercialized
Commercial and Web
Short description
CLX3 Wall Bracket
Medium description
Wall bracket for CLX3 cantilevers
Material
Steel
Material type or surface treatment
Pre-galvanized
Environmental corrosion class
C2
Base
Activity
Cable support systems
Product family
Support system
Brand
Wibe
Range
clx3
GTIN
7321677958047
ETIM (EC000022-Bracket for cable support system)
Length (EF001438)
163 mm
Width (EF000008)
101 mm
Height (EF000040)
26 mm
Suitable for cable management system width (EF008339)
100 - 600 mm
Model (EF000010)
Other
Angle (EF005434)
* °
Load bearing capacity (EF002918)
* kN
Suitable for circuit integrity (EF007806)
No
Material (EF002169)
Steel
Material quality (EF001257)
*
Surface protection (EF000139)
Continuously galvanized
Colour (EF000007)
*
RAL (EF000116)
*
Logistic
Pack 1 type
Each
Quantity pack 1
1
Length pack 1
163 mm
Width pack 1
101 mm
Height pack 1
26 mm
GTIN pack 1
7321677958047
Pack 4 type
Pallet
Quantity pack 4
182
Weight pack 4
95 kg
Length pack 4
1200 mm
Width pack 4
800 mm
Height pack 4
340 mm
Customs code
73089059
Net weight
0.31 kg
Country of origin
SE
Certification
ETIM class
EC000022
Product downloads
Environmental Documents
Corrosion class | C1 | C2 | C3 | C4 | C5 | CX | |
Environmental corrosion | Very low | Low | Average | High | Very high | Extreme | |
Examples of environments | Indoors | Heated areas with arid atmosphere and insignificant quantities of pollutant, e.g. offices, shops, schools and hotels. | Non-heated areas with fluctuating levels of temperature and humidity. Few instances of condensation and low levels of airborne pollution, e.g. sports halls and warehouses. | Average levels of humidity and some airborne pollution resulting from production processes, e.g. breweries, dairies, laundries. | High humidity and considerable airborne pollution as the result of production processes, e.g. chemical plants, swimming pools and dockyards. | Buildings with almost permanent condensation and with high pollution | Industrial buildings with extreme humidity and aggressive atmosphere. |
Outdoors | Atmospheres with low levels of airborne pollution. Rural areas. | Atmospheres containing some salt or average levels of air-borne pollution. Urban and light industrial areas. Areas affected by coastal conditions. | Atmospheres with average salt content or discernible levels of airborne pollution. Industrial and coastal areas. | Industrial areas with high humidity and aggressive atmosphere, and coastal areas with high salinity | Offshore areas with high salinity, industrial areas with extreme humidity, and aggressive atmospheres, sub-tropical or tropical atmospheres. | ||
Wibe Group designation
Exceeds requirements. Extremely high durability.
Recommended very high durability ( >20 years)
Possible alternative. High durability (10-20 years) |
Electro-galvanized (EG) |
|
|
||||
Pre-galvanized (PG) |
|
|
|
||||
Zinc+ (Z+) |
|
|
|
|
|||
Hot-dip galvanized (HDG) |
|
|
|
|
|
||
Zinkpox (ZP) |
|
|
|
|
|
|
|
Stainless steel AISI 304L(SS304) |
|
|
|
|
|
|
|
Stainless steel AISI 316L (SS316) |
|
|
|
|
|
|
|
Glass Fibre Reinforced Polymer (FRP/GRP) |
|
|
|
|
|
|
This table shows estimated values.
For more detailed advice, please contact technical support at Wibe Group